Combined Torsion in Reinforced Concrete L-Beams with Stirrups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Combined Torsion in Reinforced Concrete L-Beams with Stirrups

Author(s): Huey Ming Liao and Phil M. Ferguson

Publication: Journal Proceedings

Volume: 66

Issue: 12

Appears on pages(s): 986-993

Keywords: beams (supports) ; bending; bendingmoments; combined stress; cracking (fracturing) ;interaction diagram; L-beam; reinforced concrete;reinforcing steels; research; shear properties;

DOI: 10.14359/7447

Date: 12/1/1969

Abstract:
Exploratory tests on L-beams with closed-stirrup reinforcement and subjected to pure torsion, to torsion with moment, and to combined torsion, shear, and moment are reported. Stirrups were found to be efficient in adding strength, but large rotations were necessary to develop the added strength. Where longitudinal steel is ample, Ersoy’s circular interaction diagram between torsion and shear still seems applicable with the increased strengths. The indication is that present design procedures are conservative as to strength.