Some Field Experience in the Use of an Accelerated Method of Estimating 28-day Strength of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some Field Experience in the Use of an Accelerated Method of Estimating 28-day Strength of Concrete

Author(s): V. M. Malhotra and N. G. Zoldners

Publication: Journal Proceedings

Volume: 66

Issue: 11

Appears on pages(s): 894-897

Keywords: accelerated tests; compressive strength; concretes; quality control; tests.

DOI: 10.14359/7437

Date: 11/1/1969

Abstract:
Statistically analyzes field strength data supplied by various organizations using the accelerated method of estimating 28-day strength of concrete. Briefly, the accelerated* method consists of initial standard moist-curing of test specimens for 24 hr, followed by boiling for 31/2 hr, and testing in compression I hr later. The analyses of the test data indicate that the accelerated test method under discussion is an excellent means for rapid strength determination of concrete, and its use by the concrete industry is recommended.