Eccentrically Loaded Concrete Columns Under Sustained Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Eccentrically Loaded Concrete Columns Under Sustained Load

Author(s): R. Green and John E. Breen

Publication: Journal Proceedings

Volume: 66

Issue: 11

Appears on pages(s): 866-874

Keywords: axial loads; bending moments: columns (supports) ; creep properties: deflection; eccentric loads; reinforced concrete; research;stress-strain relationships.

DOI: 10.14359/7434

Date: 11/1/1969

Abstract:
An experimental investigation into the sustained load response of 10 eccentrically loaded unrestrained reinforced concrete columns is reported, Primary interest was in their axial load-moment-curvature- time behavior. Midheight moments and curvatures increased with time, and had not reached limiting values after 115 years of sustained load. Two columns loaded up to 160 percent of service load became unstable within 2 months of loading. The Hognestad stress-strain diagram as usually modified for long-time loading underestimates time-dependent curvatures for a given moment for small sections.