Title: Dynamic Behavior of Lightweight Concrete Bridges

Author(s): Mervyn J. Kowalsky, M. J. Nigel Priestley, and Frieder Seible

Publication: Structural Journal

Volume: 97

Issue: 4

Appears on pages(s): 602-618

Keywords: bridges; dynamic loading; lightweight concrete; seismic design.

DOI: 10.14359/7426

Date: 7/1/2000

Abstract:
The research described in this paper considers the effect of dynamic response on lightweight concrete bridge members as related to shear and flexural behavior. A series of shake-table tests were conducted and the results presented that provide further support for a previous study by the authors on the cyclic behavior of lightweight concrete bridges.