Strengthening Reinforced Concrete Beams Using Fiber Reinforced Polymer (FRP) Laminates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strengthening Reinforced Concrete Beams Using Fiber Reinforced Polymer (FRP) Laminates

Author(s): N. F. Grace, G. A. Sayed, A. K. Soliman and K. R. Saleh

Publication: Structural Journal

Volume: 96

Issue: 5

Appears on pages(s): 865-875

Keywords: ductility; reinforced concrete; strengthening

DOI: 10.14359/741

Date: 9/1/1999

Abstract:
The behavior of reinforced concrete beams strengthened with various types of fiber reinforced polymer (FRP) laminates is presented in this paper. The experimental program included strengthening and testing 14 simply supported rectangular cross section beams. Each beam was initially loaded above its cracking load. The cracked beams were strengthened with FRP laminates and then tested until complete failure. Five available strengthening systems of various types of car-bon/glass fiber reinforced polymer (CFRP/GFRP) strengthening materials were used. These materials included two types of CFRP sheets, bi- and unidirectional GFRP sheets, and CFRP plates. The effects of strengthening on deflection, failure load and failure mode, strain, and beam ductility are discussed. In addition, the influence of different numbers of FRP layers, type of epoxy, and strengthening pattern on the behavior of beams was examined. The ratio of absorbed energy at failure to total energy, or energy ratio, was used as a measure of beam ductility. It is concluded that, in addition to the longitudinal layers, the fibers oriented in the vertical direction forming a U-shape around the beam cross section significantly reduce beam deflections and increase beam load carrying capacity. Furthermore, the presence of vertical FRP sheets along the entire span length eliminates the potential for rupture of the longitudinal sheets. The combination of vertical and horizontal sheets, together with a proper epoxy, can lead to a doubling of the ultimate load carrying capacity of the beam. However, all the strengthened beams experienced brittle failure, mandating a higher factor of safety in design.