Selection and Use of Materials for Precast Concrete Wall Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Selection and Use of Materials for Precast Concrete Wall Panels

Author(s): ACI Committee 533

Publication: Journal Proceedings

Volume: 66

Issue: 10

Appears on pages(s): 814-819

Keywords: accelerating agents; admixtures; aggregates; air entrainment; architectural concrete; colors (materials) ; concrete panels; exposed aggregate concrete; finishes; formwork (construction) ; form liners;insulation;joint sealers;pigments; portland cements.

DOI: 10.14359/7408

Date: 10/1/1969

Abstract:
Presents recommendations for selection and use of the following in the production of precast concrete panels: (1) portland cement; (2) back-up concrete aggregates; decorative facing aggregates; (4) concrete admixtures; (5) reinforcement; forming materials; (7) jointing materials; (8) insulation; and (9) protective coatings. This is the second installment of a four-part series by Committee 533; future recommendations will cover design of panels and their fabrication; handling, and erection.