Yield Line Analysis of Slabs supported on Three Sides

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Yield Line Analysis of Slabs supported on Three Sides

Author(s): Edward C. Demsky and David S. Hatcher

Publication: Journal Proceedings

Volume: 66

Issue: 9

Appears on pages(s): 741-744

Keywords: bending moments; concrete slabs; loads (forces) ; reinforced concrete; reinforcing steels; yield line method.

DOI: 10.14359/7397

Date: 9/1/1969

Abstract:
Yield line solutions for the collapse load of isotropic and non-isotropic slabs supported on three sides were obtained. The loading varied from uniform to a triangular distribution with zero load at the free edge. The effects of aspect ratio, reinforcement arrangement, and loading on the collapse load were studied. Mechanisms with and without corner levers were studied and the reduction in the collapse due to corner levers was determined. The relative economy of various reinforcement arrangements was studied.