Lateral Load Analysis of Multistory Structures Comprising Shear Walls With Sudden Changes in Stiffness

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lateral Load Analysis of Multistory Structures Comprising Shear Walls With Sudden Changes in Stiffness

Author(s): Jacob Gluck

Publication: Journal Proceedings

Volume: 66

Issue: 9

Appears on pages(s): 729-736

Keywords: deflections; lateral pressure: loads (forces) multistory buildings; reinforced concrete; shear walls; stiffness; structural analysis.

DOI: 10.14359/7395

Date: 9/1/1969

Abstract:
A practical manual method is presented for determining the lateral load distribution in multi-story structures comprising shear walIs symmetrically arranged in plan, with sudden changes in stiffness. The proposed method consists of two parts: in the first (basic solution), the load distribution is determined on the assumption of a common deflection line, continuous throughout the height of the structure-: in the second, a correction (complementary solution) is applied, taking into account that the deflections of the shear walls are only equalized at floor levels.