Recommended Practice for Concrete Floor and Slab Construction (ACI 302-69)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommended Practice for Concrete Floor and Slab Construction (ACI 302-69)

Author(s): ACI Committee 302

Publication: Journal Proceedings

Volume: 66

Issue: 8

Appears on pages(s): 609

Keywords: ACI standard; admixtures (concrete) ; aggregates; concrete; consolidation; construction; cracking (fracture) ; curing; driveways; durability; floor toppings; floors;heavy duty floors;inspection;joints;mix proportioning;patios;placing;quality control.

DOI: 10.14359/7383

Date: 8/1/1969

Abstract:
Quality of a concrete slab or floor is highly dependent on achieving a hard and durable surface which is plane and free of cracks. The properties that the surface has are determined by the quality of the concreting operations. Furthermore, timing of these concreting operations and finishing techniques is critical. Otherwise, undesirable changes occur at the wearing surface; these may lead to soft or dusting surfaces, permeable concrete, cracking, and poor durability. This recommended practice tells how to produce good quality floors and slabs for various classes of service, emphasizing such aspects of construction as site preparation, concreting materials, concrete mixture proportions, concreting, workmanship, and curing. Adequate supervision and inspection are required of all job operations including particularly those of finishing.