Title: Analysis of Reinforced Concrete Columns Subjected to Longitudinal Load and Biaxial Bending

Author(s): Anis Farah and M. W. Huggins

Publication: Journal Proceedings

Volume: 66

Issue: 7

Appears on pages(s): 569-603

Keywords: bending; biaxial loads; columns (supports); loads (forces) ; reinforced concrete; structural analysis.

DOI: 10.14359/7382

Date: 7/1/1969

Abstract:
Analyzes hinged reinforced concrete columns subjected to biaxial bending. The integration method used in the analysis leads to three simultaneous nonlinear equations which are solved by a procedure based on the Newton-Raphson method. An example is solved and the results are compared with those obtained from experiment. The agreement is exceptionally good.