Shear Capacity of Lightweight Concrete Flat Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Capacity of Lightweight Concrete Flat Slabs

Author(s): Charles B. Ivy, Don L. Ivey, and Eugene Buth

Publication: Journal Proceedings

Volume: 66

Issue: 6

Appears on pages(s): 490-493

Keywords: concrete slabs; lightweight aggregate concretes; lightweight aggregates; reinforced concrete; research; shear strength; splitting tensile strength; structural design.

DOI: 10.14359/7376

Date: 6/1/1969

Abstract:
Fourteen full scale lightweight concrete slabs were tested to provide additional information concerning the resistance of lightweight structural concrete to shear. Since the shear requirements for this type of structure in ACI 318-63 were based on a total of six slab tests, it was considered desirable to supplement this information in order to evaluate or propose modifications to the Code. Slab test results are compared to the shear requirements of ACI 318-63 and to other design approaches that are under consideration as modifications or changes to these requirements.