Tests to Failure in Bending and Torsion of Reinforced Concrete Bents

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests to Failure in Bending and Torsion of Reinforced Concrete Bents

Author(s): V. Ramakrishnan and Y. Ananthanarayana

Publication: Journal Proceedings

Volume: 66

Issue: 5

Appears on pages(s): 428-443

Keywords: beams (supports) ; bending: bents;flexural tests; frames; interaction curves; limit design method (structural) ; reinforced concrete; research; structural design; torsion.

DOI: 10.14359/7371

Date: 5/1/1969

Abstract:
Presents the results of an analytical investigation into the experimental and ultimate strength capacity of I2 reinforced concrete right angle bents fixed at each end and subjected to a single concentrated load. Sixteen reinforced concrete beams having the same cross-sectional properties as the bents were also tested in flexure, torsion, and combined flexure and torsion to obtain the applicable interaction relation between the bending and twisting strengths of the section. The analytically computed collapse loads obtained on the basis of this interaction relationship and the experimental collapse loads of the bents are compared. Some design recommendations are suggested. .