Title: Crack Control in One-Way Slabs Reinforced with Deformed Welded Wire Fabric

Author(s): John P. Lloyd, Hassen M. Rejali, and Clyde E. Kesler

Publication: Journal Proceedings

Volume: 66

Issue: 5

Appears on pages(s): 366-376

Keywords: concrete slabs; crack propagation; crack width and spacing; cracking (fracturing); reinforcement; reinforced concrete; reinforcing steel; research; welded wire fabric.

DOI: 10.14359/7363

Date: 5/1/1969

Abstract:
Twenty-three one-way slabs reinforced with either deformed wire, deformed bar, or deformed welded wire fabric were tested by third-point loading. The crack controlling abilities of the three types of reinforcements were compared with one another. The results were also compared to those of other researchers. This study indicated that deformed wires, deformed bars, and deformed welded wire fabric control crack spacings and crack widths equally well when placed similarly.