Computer Study of Long Columns in Frames

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computer Study of Long Columns in Frames

Author(s): Phil M. Ferguson, Hajime Okamura, and Shriniwas N. Pagay

Publication: Journal Proceedings

Volume: 67

Issue: 12

Appears on pages(s): 955-958

Keywords: buckling; columns (supports) ; frames;long columns; reinforced concrete; structural design.

DOI: 10.14359/7327

Date: 12/1/1970

Abstract:
An extensive computer study of long column action in frames is summarized for both unbraced and braced building frames. This summary paper (1) indicates the weakness of the R-method in caring for column buckling in certain frames subject to sidesway, (2) compares the accuracy of the moment magnifier and R-methods in this and other situations, and (3) gives the background for the modified R equations mentioned as alternates in the explanation of changes of the Building Code.