Title: Opportunities in Bond Research

Author(s): ACI Committee 408

Publication: Journal Proceedings

Volume: 67

Issue: 11

Appears on pages(s): 857-867

Keywords: anchorage (structural) ; bond (concrete to reinforcement) ; , bond stress; connections; deformations (reinforcing steal) ; failure mechanics; fatigue tests; lightweight aggregate concretes;prestressed concrete;reinforced concrete; reinforcing steels.

DOI: 10.14359/7315

Date: 11/1/1970

Abstract:
Based on a survey of some of the many unsolved problems of concrete-to-steel bond behavior, suggestions are given for possible research on several subject-mode of failure, joint details, reinforcement deformations, bond fatigue in reinforced concrete, bond of nonprestressed reinforcement in lightweight concrete, bond in prestressed concrete, bond of wire and fabric, and splices.