Stresses in Flat Plates Near Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stresses in Flat Plates Near Columns

Author(s): Paul E. Mast

Publication: Journal Proceedings

Volume: 67

Issue: 10

Appears on pages(s): 761-768

Keywords: axial loads; bending moments; columns (supports) ; elastic limit; flat concrete plates; flexural strength; plate load tests; reinforced concrete; shear strength; static tests; structural analysis;theory of elasticity;torsion.

DOI: 10.14359/7306

Date: 10/1/1970

Abstract:
An analytical method is presented to determine the stresses in flat plates near columns. It is based on the flexural theory of elastic plates. The method takes into account the shape of the column and the dimensions and boundary conditions of the plate. The analytical values thus obtained are com-pared with the corresponding values obtained by other methods. Perfect agreement exists with more elaborate methods based on plate theory. Concerning approximate methods, theoretical inconsistences are pointed out to explain the differences in results. The analytical values, furthermore, are compared with test results and good agreement can be realized. Simplified formulas are suggested for design purposes.