Influence of Cement Composition on the Creep of Concrete Containing Admixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Cement Composition on the Creep of Concrete Containing Admixtures

Author(s): Brian B. Hope and Noel H. Brown

Publication: Journal Proceedings

Volume: 67

Issue: 9

Appears on pages(s): 673-674

Keywords: admixtures; cement pastes; compression;compressive strength; concretes; creep properties;C3A; gels; modulus of elasticity; portland cement compund composition;portland cements;retardents;water-reducing agents;workablity.

DOI: 10.14359/7304

Date: 9/1/1970

Abstract:
The creep of plain concrete was compared with that of concrete containing two water-reducing and set-retarding admixtures. Four cements of different tricalcium aluminates content were used and specimens were loaded in compression at 7 and 28 days to a stress/strength ratio of 0.3. Admixtures modified the rate of creep. The change in total creep over the test period varied from a decrease of 30 percent to an increase of 30 percent depending on the age at which the load was applied and the admixture and cement used. Although creep is affected by varying the C3A content, other factors in cement composition appear to be influential since no definite trends could be observed.