Specifications for Cast-in-Place Nonreinforced Concrete Pipe (ACI 346-70)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Specifications for Cast-in-Place Nonreinforced Concrete Pipe (ACI 346-70)

Author(s): ACI Committee 346

Publication: Journal Proceedings

Volume: 67

Issue: 6

Appears on pages(s): 441

Keywords: admixtures (concrete); aggregates; air enterainment; cast-in-place pipe; compressive strength; concrete construction; concrete pipe; concretes; curing; finishing; formwork (construction); joints; mixing; mix proporitioning; patching; placing repairs.

DOI: 10.14359/7282

Date: 6/1/1970

Abstract:
These specifications are a reference standard which the engineer or architect may make applicable to any cast-in-place pipe project by citing them in the project specifications. Individual chapters or sections should not be copied into project specifications. Individual chapters or sections should not be copied into project specifications since their meanings will be changed by taking them out of context. The specifications need to be supplemented by designating or specifying individual project requirements. A list is provided indicating places in these specifications and items that will require, or may require, specific treatment by the specification writer.