Analysis of Shrinkage Effects on Reinforced Concrete Structural Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of Shrinkage Effects on Reinforced Concrete Structural Members

Author(s): Robert H. Elvery and Muhamed Shafi

Publication: Journal Proceedings

Volume: 67

Issue: 1

Appears on pages(s): 45-52

Keywords: beams (supports) ; deflection; reinforced concrete; shrinkage; stresses; structural analysis; warpage.

DOI: 10.14359/7257

Date: 1/1/1970

Abstract:
Analyzes the structural behavior of reinforced concrete members under normal conditions of drying to predict stresses and deformations. The theoretical determination of curvature so obtained shows good agreement with experimental results obtained by the authors and also with those reported in the literature. This investigation indicates in particular that the deflection of some reinforced concrete beams due to shrinkage can be of appreciable magnitude for spans greater than about 40 ft.