Title: Deep Beam Behavior Affected by Length and Shear Span variations,”

Author(s): Robert F. Manuel, Bruce W. Slight, Gerhard T. Suter

Publication: Journal Proceedings

Volume: 68

Issue: 12

Appears on pages(s): 954-958

Keywords: Cracking (fracturing), crack width and spacing, deep beams, deflection, failure, reinforced concrete, research, strains

DOI: 10.14359/7246

Date: 12/1/1971

Abstract:
Summarizes results of investigations of 12 reinforced concrete deep beams in which variables a/d and L/d systemically varied and other major variables kept constant