Title: Design Factors for the Equivilent Frame Method

Author(s): Sidney H. Simmonds, Janko Misic

Publication: Journal Proceedings

Volume: 68

Issue: 11

Appears on pages(s): 825-831

Keywords: Bending moments, concrete slabs, moment distributuion, reinforced concrete, structural analysis

DOI: 10.14359/7242

Date: 11/1/1971

Abstract:
Requirements of ACI 318-l 7 considered in providing simplification of method for calculation of stiffness for slab-beam and column elements.