Plain and Reinforced Concrete L-Beams Under Combined Flexure, Shear, and Torsion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Plain and Reinforced Concrete L-Beams Under Combined Flexure, Shear, and Torsion

Author(s): P. K. Syamal, M. S. Mirza and D. P. Ray

Publication: Journal Proceedings

Volume: 68

Issue: 11

Appears on pages(s): 848-860

Keywords: Beams (suports), bending, cracking (fracturing), interaction diagrams, L-beams, plain concrete, reinforced concrete, research, shear properties, torsion

DOI: 10.14359/7239

Date: 11/1/1971

Abstract:
Results of tests on 33 L-beams subjected to combined bending, shear, torsion. Interaction curves and interaction surfaces constructed from experimental results.