Preparation of Notation for Concrete (ACI 104-71)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Preparation of Notation for Concrete (ACI 104-71)

Author(s): ACI Committee 104

Publication: Journal Proceedings

Volume: 68

Issue: 9

Appears on pages(s): 645

Keywords: Coding, concretes, definitions, nomen-clature, precast concrete, reinforced concrete, structural analysis, structural design, symbols

DOI: 10.14359/7237

Date: 9/1/1971

Abstract:
Adopted as a standard, indicates how symbols shall be selected to represent quantities or terms. Principal sym-bols are upper and lower case Roman letters and Greek lower case letters, with Roman lower case used as sub-scripts. Greek capital letters are reserved for mathematics.