Guide for Use of Admixtures in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide for Use of Admixtures in Concrete

Author(s): ACI Committee 212

Publication: Journal Proceedings

Volume: 68

Issue: 9

Appears on pages(s): 646-676

Keywords: Accelerating agents, admixtures, air-entraining agents, alkali-aggregate reactions, aluminum powder, bactericides, batching, calcium chlorides, colors (materials), con-crete durability,

DOI: 10.14359/7236

Date: 9/1/1971

Abstract:
Revises earlier standard, discusses preparation, air-entrainment, accelerating, water-reducing and set-controlIing, finely divided m inera I admixtures.