Flexure of Reinforced Concrete Beams With Confined Compression Zones

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexure of Reinforced Concrete Beams With Confined Compression Zones

Author(s): K. T. Sundra Raja Iyengar, Prakash Desayi, and K. Nagi Reddy

Publication: Journal Proceedings

Volume: 68

Issue: 9

Appears on pages(s): 719-725

Keywords: Beams (supports), confined concrete, deflec-tion, ductility, flexural strength, reinforced concrete, research, spiral reinforcement, stress block, stress-strain relationship, struc-tural design, ultimate strength

DOI: 10.14359/7234

Date: 9/1/1971

Abstract:
Presents the development of stress blocks and a flexural analysis of reinforced concrete sections with compression concrete confined in circular spiral steel binders. Results of 18 reinforced concrete beams tested by authors and 30 beam tests available in the literature are analyzed by the proposed method and a satisfactory agreement found between the computed and the experimental ultimate moment.