Title: Diagonal Crack Width Control in Short Beams

Author(s): Gerhard T. Suter and R. F. Manuel

Publication: Journal Proceedings

Volume: 68

Issue: 6

Appears on pages(s): 451-455

Keywords: Beams (support), brackets, crack width, cracking (fracturing), deflection, reinforced concrete, k stirrups; wc b reinforcement

DOI: 10.14359/7202

Date: 6/1/1971

Abstract:
Short beam test results indicate beams containing no web reinforcement develop diagonal crack widths at working load levels may present a serious serviceability problem. Control of the serviceability problem and simultaneous attainment of flexural capacity requires only a single verti-cal or inclined stirrup. Twelve short, reinforced concrete beams tested in an effort to define control measures with minimum web reinforcement.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer