Compaction of Concrete Slabs by Vibration

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compaction of Concrete Slabs by Vibration

Author(s): Leland M. Kraft, Jr.

Publication: Journal Proceedings

Volume: 68

Issue: 6

Appears on pages(s): 462-467

Keywords: Air entrainment; coarse aggregates, concrete pavements, concrete slabs, consolidation, vibration

DOI: 10.14359/7199

Date: 6/1/1971

Abstract:
Large air and water pockets observed in cores taken from well vibrated concrete pavements studied, indicating several para-meters may influence volume of entrapped air in thin concrete sections compacted with spud vibration. Results suggest use of surcharge may be beneficial in reducing entrapped air, and that crushed stone concrete mixes may yield lower air content than round stone.