Title: Slab Foundation Subjected to Complex Loads

Author(s): John J. Panak, David W. Fowler, and Hudson Matlock

Publication: Journal Proceedings

Volume: 69

Issue: 10

Appears on pages(s): 630-639

Keywords: Bending moments, computer programs, concrete slabs, deflection, foundations, loads (forces), reinforced concrete, structural design

DOI: 10.14359/7184

Date: 10/1/1972

Abstract:
Paper describes complex loading design and of continuous foundations with geometry.