Underwater Transporting of Concrete With the Hydro-Valve

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Underwater Transporting of Concrete With the Hydro-Valve

Author(s): Louis C. Schoewert and Henri F. Hillen

Publication: Journal Proceedings

Volume: 69

Issue: 9

Appears on pages(s): 584-588

Keywords: Concrete construction, concrete, construction equipment, placing, reinforced concrete, under- water construction

DOI: 10.14359/7180

Date: 9/1/1972

Abstract:
Describes method developed in the Netherlands for placing concrete under water. Device allows placing concrete of higher quality, provides means of placing reinforced concrete.