Analysis of Reinforced Concrete Membrane Subject to Tension and Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of Reinforced Concrete Membrane Subject to Tension and Shear

Author(s): Nicholas B. Dunchon

Publication: Journal Proceedings

Volume: 69

Issue: 9

Appears on pages(s): 578-583

Keywords: Cracking (fracturing), deformation, finite element method, pressure vessels, pre- stressed concrete, reinforced concrete, shear stress, structural analysis

DOI: 10.14359/7179

Date: 9/1/1972

Abstract:
Analytical procedure presented to predict stresses and deformations in reinforced or prestressed concrete walls subjected to membrane forces, and reinforced by combination of orthogonal and inclined bars.