Title: Fire Endurence of Selected Concrete Masonry Walls

Author(s): L.W. Allen and T.Z. Harmathy

Publication: Journal Proceedings

Volume: 69

Issue: 9

Appears on pages(s): 562-568

Keywords: Aggregates, autoclaves, concrete blocks, concrete, expanded clay aggregates, fire resistance, lightweight aggregate concretes, research, thermal properties

DOI: 10.14359/7177

Date: 9/1/1972

Abstract:
Walls made from 44 different types of concrete masonry units subjected to fire endurance tests. Three semi-empirical formulas used to express fire endurance with these walls as a function of three geometric variables and two thermal properties characterizing the shape and material of constituent masonry units.