A Design Procedure for Continuously Reinforced Concrete Pavements for Highways pavements for highways,”

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Design Procedure for Continuously Reinforced Concrete Pavements for Highways pavements for highways,”

Author(s): ACI Committee 325

Publication: Journal Proceedings

Volume: 69

Issue: 6

Appears on pages(s): 309-319

Keywords: Anchorage (structural), concrete pavements, continuity (structural), continiously rein-forced pavements, flexural strength, joints

DOI: 10.14359/7157

Date: 6/1/1972

Abstract:
Presents interim design method based on current practices for determining pavement thickness and amount of reinforcing steel for continuously reinforced concrete pavement. Also gives recommendations for end anchorage systems. Pavement thickness design method based on modificaitons of design equations presented in AASHO interim guide prepared after completion of road tests in Illinois.