Recommended Practice for Hot Weather Concreting (ACI305-72)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommended Practice for Hot Weather Concreting (ACI305-72)

Author(s): ACI Committee 305

Publication: Journal Proceedings

Volume: 69

Issue: 5

Appears on pages(s): 261

Keywords: Admixtures, aggregates, bleeding (concrete); compressive strength, concrete construction, concrete finishing (fresh concrete), cooling, curing, hot weather construction, joints

DOI: 10.14359/7155

Date: 5/1/1972

Abstract:

Note: This journal article is only a ONE page abstract for 305-72. To purchase the entire .pdf, please contact our Customer Service Center at (248) 848-3800 or bkstore@concrete.org

Adopted at ACI 30572 Standard, describes concrete mixed, transported, and placed under conditions of high temperature, low humidity, or wind. Recommended practice defines hot weather, lists possible unfavorable effects and recommends practices intended to minimize them. Includes a selected bibliography.