Title: Responsibility for Inspection

Author(s): Dixon O'Brien, Jr. and Bertold E. Weinberg

Publication: Journal Proceedings

Volume: 69

Issue: 6

Appears on pages(s): 320-333

Keywords: Concrete construction, concretes, con-struction costs, inspection, laboratories, quality control, reinforced concrete, specifications, structural design, tests

DOI: 10.14359/7154

Date: 6/1/1972

Abstract:
Five papers based on session sponsored by ACI committee 311 -- Inspection of Concrete, and 348 - - Structural Safety, at 1971 fall convention in Buffalo. Includes Corps of Engineers approach to contractor quality control, Owners viewpoint of responsibility for construction quality control, Incomplete inspection the designer's dilemma, Inspection and quality control in concrete construction a contractor’s viewpoint, and Quality assurance systems by the independent testing agency.