Decision Logic Table Format For Building Code Requirements for Reinforced Concrete (ACI 318-71)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Decision Logic Table Format For Building Code Requirements for Reinforced Concrete (ACI 318-71)

Author(s): ACI Committee 118

Publication: Journal Proceedings

Volume: 70

Issue: 12

Appears on pages(s): 788-794

Keywords: building codes; computation; computer logic; computers; decision theory; decisions; mathematical logic; structural analysis; structural design.

DOI: 10.14359/7142

Date: 12/1/1973

Abstract:
The basic concepts of decision logic tables and their application as a format for the presentation of the reinforced concrete building design code are discussed. Sections 3.3.2, 12.5 and 9.3.1-9.3.3 of ACI 318-71 are presented in decision logic table format as examples.