Strain Factors and Moment Factors for Singly and Doubly Reinforced Beams Under Repeated l o a d i n g

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strain Factors and Moment Factors for Singly and Doubly Reinforced Beams Under Repeated l o a d i n g

Author(s): V. S. Thattey

Publication: Journal Proceedings

Volume: 72

Issue: 12

Appears on pages(s): 727-730

Keywords: beams (supports); bending; compression; deflec- tion; loads (forces); moments; reinforced concrete; strains; stress-strain relationships; tension.

DOI: 10.14359/7070

Date: 12/1/1975

Abstract:
Reports on an investigation of the response of simply supported singly and doubly reinforced beams to arbitrary. repeated loading. A numerical method using load deflection relationship for computing strain factors at various stages of loading is proposed. Moment factor equations are devel-oped involving the parameters like modular ratio, per-centage reinforcement, ratio of compression steel area to tension steel area, strain factor, and stress ratio. The theo-retical and experimental comparison indicates that the theoretical equations involving strain factors may give a rough indication of the behavior of reinforced concrete beams under repeated loading. [Authors]