Transfer and Development Lengths of Carbon Fiber Reinforced Polymers Prestressing Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Transfer and Development Lengths of Carbon Fiber Reinforced Polymers Prestressing Reinforcement

Author(s): Zaki I. Mahmoud, Sami H. Rizkalla, and Ezz-Eldin R. Zaghoul

Publication: Structural Journal

Volume: 96

Issue: 4

Appears on pages(s): 594-602

Keywords: carbon; fiber; polymers; prestressing; reinforcing materials; stress transfer

DOI: 10.14359/696

Date: 7/1/1999

Abstract:
Fundamental understanding of the behavior and specific characteristics of fiber reinforced polymers (FRP) prestressing tendons such as bond strength, transfer, and development lengths are of prime importance for the development of design guidelines and codes for concrete structures prestressed with FRP reinforcements. This paper is a continuation of the paper published in the May-June 1998 ACI Structural Journal entitled “Bond Properties of Carbon Fiber Composite Prestressing Strands.” In this study, the results of 52 tested specimens are used to determine the transfer and development length of two types of carbon fiber reinforced polymers (CFRP). The reinforcements used in this study are Leadline bars, carbon fiber composite cables (CFCC), and steel strands used for control specimens. The new configuration of the concrete prism used in this study is proposed as a standard test to evaluate the transfer and development lengths of FRP prestressing reinforcements. The effect of concrete confinement, simulating the effect of shear reinforcement, on the transfer and flexural bond lengths is included. Effect of shrinkage and creep of concrete on the transfer length is also reported. Based on the experimental results, design models are proposed to predict the transfer and flexural bond lengths of Leadline and carbon fiber composite cables.