New Corrosion Protection System for Concrete Structures Using a Newly Developed Alloy

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Corrosion Protection System for Concrete Structures Using a Newly Developed Alloy

Author(s): M. Funahashi, W. T. Young, M. R. Tighe, S. F. Daily and C. Firlotte

Publication: Symposium Paper

Volume: 170

Issue:

Appears on pages(s): 555-570

Keywords: Cathodic protection; chlorides; concretes; corrosion; galvanic corrosion.

DOI: 10.14359/6841

Date: 7/1/1997

Abstract:
Maintenance costs for concrete structures that are exposed to de-icing salts and marine environments represent large expenditures for owners as a results of corrosion of steel in concrete. To solve this problem, the US Federal Highway Administration sponsored a comprehensive program todevelop a new alloy to be used as a sacrificial anode for reinforced and prestressed concrete structures. Based on intensive studies of existing metals and alloys, a new alloy was developed to overcome the observed deficiencies in the existing materials. The new aluminum-zinc alloy can be thermally sprayed on concrete surfaces to protect steel from corrosion in chloride contaminated concrete. This paper presents the results of both laboratory testing and field installation of this new alloy.