Effect of Fly Ash and Corrosion inhibitor on Reinforced Concrete in Marine Environments

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Fly Ash and Corrosion inhibitor on Reinforced Concrete in Marine Environments

Author(s): Chau Lee and M.G.Lee

Publication: Symposium Paper

Volume: 170

Issue:

Appears on pages(s): 141-156

Keywords: Cements; compressive strength; corrosion; electrical properties; expansion; fly ash.

DOI: 10.14359/6820

Date: 7/1/1997

Abstract:
The corrosion resistance of reinforced concrete, containing fly ash and calcium nitrite-based corrosion inhibitor, under sea water attack was studied in this research. Aggressive and normal construction conditions were simulated. Test results indicate that the use of calcium nitrite-based corrosion inhibitor is an effective way to protect reinforcing steel from corrosion in aggressive environments. No serious detrimental effect was found for the corrosion inhibitor on concrete properties. Replacement of 20% cement by fly ash gives no apparent improvement in preventing the corrosion of steel in sea water exposure.