Dry-Mix Shotcrete Practice

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Dry-Mix Shotcrete Practice

Author(s): Theodore R. Crom

Publication: Symposium Paper

Volume: 14

Issue:

Appears on pages(s): 15-32

Keywords:

DOI: 10.14359/6802

Date: 3/1/1978

Abstract:
Describes the techniques of dry-mix shotcreting. Cements and aggregates for shotcrete are reviewed. Basic types of equipment manu-factured in the United States are discussed, and their operation is explained, including details of the nozzleman’s work. Sand pockets are defined, and reasons for avoiding such imperfections are given. Recommendations on the use, size, and proper en-casement of reinforcing steel are made. Bonding ability, curing, finishing, and acceptable weather conditions for shotcreting are considered. Comments are given regarding compressive strength testing and qualification of nozzlemen.