Techniques for In-Plane Vibration and Shear Testing of Model Floor Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Techniques for In-Plane Vibration and Shear Testing of Model Floor Slabs

Author(s): H.Faruk Karadogan,Le-Wu Lu, and Ti Huang

Publication: Symposium Paper

Volume: 73

Issue:

Appears on pages(s): 189-204

Keywords: concrete slabs; cyclic loads; elastic analysis; epoxy resins; floors; lateral loads; loads (forces); models; repairs; shear strength; shear tests; stiffness; vibration tests. --

DOI: 10.14359/6780

Date: 3/1/1982

Abstract:
Small size models of two concrete floor systems have been tested for their elastic and post-elastic behavior under in-plane shear action. Parameters studied include cyclic and monotonic loading, shear span aspect ratio, effect of gravity load and repair by epoxy injection method. This report describes the development of the model and techniques used in the testing. Preliminary test results and conclusions are also presented.