Beam-Column Joints: Irrational Solutions to a Rational Problem

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Beam-Column Joints: Irrational Solutions to a Rational Problem

Author(s): J. 0. Jirsa

Publication: Symposium Paper

Volume: 72

Issue:

Appears on pages(s): 177-198

Keywords: history; research; beams (supports); columns (su orts) joints (junctions); loads( forces); re specimens; structural design. ; deformation; concrete;

DOI: 10.14359/6760

Date: 12/1/1981

Abstract:
A number of approaches are available for design of beam-column joints. The joint details resulting from the application of each approach differ considerably. In most cases the transverse reinforcement required in the joint is substantial and makes fabrication difficult. The requirements for transverse reinforcement can be traced to the research which forms the basis for design rules. In many cases the loading histories used in test programs produce very large deformations which may be in excess of the deformation realized in actual structures. Research on beam-column joints is reviewed and suggestions are made for determining loading histories and test specimens which may be more rational in terms of structural performance requirements.




  