Properties of Concrete Made with Sulfate Resisting Cement and Fly Ash

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Concrete Made with Sulfate Resisting Cement and Fly Ash

Author(s): Karim W. Nasser and H.M. Marzouk

Publication: Symposium Paper

Volume: 79

Issue:

Appears on pages(s): 383-396

Keywords: compressive strength; creep properties; creep recovery; fly ash; modulus of elasticity; sulfate resisting cements. --

DOI: 10.14359/6703

Date: 5/1/1983

Abstract:
This investigation is a study of the structural properties of concrete made with sulphate-resisting cement (Type V) and Saskatchewan fly ash. Tests were performed on cylinders exposed to temperatures of 70° to 450°F (21.4° to 232°C) for periods of six months and over. The properties of strength, elasticity, creep and creep recovery were studied for both sealed and unsealed specimens. Test results revealed that temperature had a minor effect on strength and stress-strain relationship for both sealed and unsealed specimens; however, the modulus of elasticity showed a continual decrease with a rise in temperature. Creep of unsealed concrete increased with an increase in temperature up to 160°F (70°C) and decreased thereafter, while creep of sealed specimens decreased with a rise in temperature, except at 350°F (177°C) where it was one and a half times that at 70°F (21.4°