The Use of Fly Ash in Concrete-Australian Experience

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Use of Fly Ash in Concrete-Australian Experience

Author(s): A. Samarin, R.L. Munn, and J.B. Ashby

Publication: Symposium Paper

Volume: 79

Issue:

Appears on pages(s): 143-172

Keywords: reactions; abrasion resistance; air entrainment; alkali-aggregate bleeding (concrete); carbonation; compressive strength; concrete durability; creep properties,

DOI: 10.14359/6689

Date: 5/1/1983

Abstract:
The paper describes commercial use of concretes containing fly ash in Australia. comparison is made between fly ash and other concrete types, mainly on the basis of equal 28 day strength. Setting times, Bleeding, Workability, Air Entrainment, Rate of Strength Gain, Elastic Properties, Flexural and Indirect Tensile Strength, Heat of Hydration, Shrinkage Creep, Sulphate Resistance, Carbonation, Abrasion Resistance, Alkali Aggregate Reactivity are discussed. Field observations of concrete structures containing fly ash after prolonged environmental exposure are also included.