Time-Dependent Behavior of Columns in Water Tower Place

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Behavior of Columns in Water Tower Place

Author(s): H.G. Russell and W.G. Corley

Publication: Symposium Paper

Volume: 55

Issue:

Appears on pages(s): 347-374

Keywords: deformati strength strains; age; columns (supports); c on; drying shrinkage; field concretes; measurement; rein walls reep properties; creep tests; tests; high-rise buildings; high forced concrete; research;

DOI: 10.14359/6620

Date: 8/1/1978

Abstract:
An 859-ft building was instrument deformations of column of individual member displacements were measured (262 m) high reinforced concrete ted to m easure the time-dependents and walls. Vertical shortening S and their relative vertical sured at selected floor levels. Laboratory tests were the field. The elastic modulus, coefficients and shrinkage with age each different concrete laboratory tests and vertical shortening of values were compared performed on concrete obtained in iation 0f compressive strength, icient of thermal expansion, creep, of conc rete were determined for rete st rength. Based on the detailed construction records, the column S was calculated. These with those measured in the building.