A Constitutive Law for Concrete at Transient High Temperature Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Constitutive Law for Concrete at Transient High Temperature Conditions

Author(s): Y. Anderberg and S. Thelandersson

Publication: Symposium Paper

Volume: 55

Issue:

Appears on pages(s): 187-206

Keywords: tion; high temperature rise stresses compressive strength; tern erature; strains; in concrete); thermal concretes; creep properties; deforma-stress- strain relationships; tempera-expansion; thermal gradient; thermal

DOI: 10.14359/6614

Date: 8/1/1978

Abstract:
A computer-oriented constitutive model for concrete in compresslon, valid at first heating of concrete up to 800 C is described. The total deformation is expressed in terms of thermal, instantaneous stress-related, creep and transient strain components, where the transient strain is a concept introduced to describe the particular behavior under changing temperature. Comparisons with independent tests demonstrate that the material behaviour is described in a very appropriate way. The model is applied in a simple example calculation, showing that thermal stresses due to non-uniform temperature distribution are very insignificant or even nonexistant.Stresses due to restrained thermal expansion cannot in themselves contribute to compression failure of concrete.