The Interpretation of Tests on the Strength of Concrete in Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Interpretation of Tests on the Strength of Concrete in Structures

Author(s): William E. Murphy

Publication: Symposium Paper

Volume: 82

Issue:

Appears on pages(s): 377-392

Keywords: compressive strength; concrete cores; concretes; cubes; interpretation; nondestructive tests; variations.

DOI: 10.14359/6564

Date: 9/1/1984

Abstract:
The results of tests on concrete in in-situ or precast elements are only of value if they contribute to the making of valid and useful conclusions relating either to the quality of the concrete mix supplied or to the performance of the structure in service. The paper indicates how these objectives might be achieved by expressing the strength of the concrete in the structure in terms of an in-situ cube strength.