Maturity Concept Proves Effective in Reducing Form Removal Time and Winter Curing Cost

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Maturity Concept Proves Effective in Reducing Form Removal Time and Winter Curing Cost

Author(s): A.J. Hulshizer, M.A. Edgar, R.E. Daniels, J.D. Suminsby, and G.E. Myers

Publication: Symposium Paper

Volume: 82

Issue:

Appears on pages(s): 351-376

Keywords: age-strength relation; cold weather construction; -- compressive strength; concretes; costs; curing; form removal; heating; hydration; maturity meters; nondestructive tests; probes; temperature; tunnel linings.

DOI: 10.14359/6563

Date: 9/1/1984

Abstract:
Two specific areas of concrete work were identified at the Seabrook Station nuclear power plant where the knowledge of developing concrete strengths could be used to reduce cost and schedule. The Maturity Method for predicting in-situ concrete strength was evaluated under field conditions to establish it as a dependable, practical approach for the Seabrook work. Based on the test results the Maturity Method, utilizing electronic Maturity Meters, was utilized to determine concrete strengths for one application to enable tunnel arch forms to be safely removed in 12 to 14 hours and in another application to reduce winter cure heating by about 30% and shorten curing work by about two days.