Pulse Velocity as a Measure of Concrete Compressive Strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pulse Velocity as a Measure of Concrete Compressive Strength

Author(s): V.R. Sturrup, F.J. Vecchio, and H. Caratin

Publication: Symposium Paper

Volume: 82

Issue:

Appears on pages(s): 201-228

Keywords: admixtures; aggre ates; cretes; cracking (fracturing 3 compressive strength; con-; curing; density (mass/volume; freezing; moisture content; nondestructive tests; temperature; ultrasonic tests; voids.

DOI: 10.14359/6556

Date: 9/1/1984

Abstract:
Pulse Velocity/Strength relationships can be estab-lished for concrete but they are influenced by many factors. Of particular significance are the proportions and composition of the components, age s curing conditions and moisture content of the concrete. Cement type, air-entrainment and curing temperatures -influence to a lesser degree. Pulse velocity correlates well with strength at early ages but is insensitive to even major increases in strength at later ages. A relationship established at early ages therefore is not applicable as the concrete matures. A rela-tionship determined on sound concrete during its development stage cannot be used to predict the strength of concrete that is deteriorating. Such a relationship should be established on cores from the concrete in question. A relationship established using laboratory-cured specimens, cannot be used with assurance to follow strength development in a structure. A Pulse Velocity Strength relationship can be confused by cracks, voids or other discontinuities in the concrete.