Title: Verification of Structural Adequacy

Author(s): Dov Kaminetzky

Publication: Symposium Paper

Volume: 85

Issue:

Appears on pages(s): 135-156

Keywords: building; economics; evaluation; loads (forces); reinforced concrete; renovating; repairs.

DOI: 10.14359/6539

Date: 4/1/1985

Abstract:
The various steps that must be taken in order to or restored are described. After the history of the structure has been researched, a condition survey of the structure and its foundations should be performed and supplemented with a geometry Laboratory testing of material samples then follow with structural analysis carried out to determine final structural adequacy and economical feasibility. A case history is described, The paper is concluded with recommendations for the establishment of an ACI guideline and additional research.